Tamil Nadu HSE Second Year Textile Technology study materials
Tamil Nadu HSE Second Year Textile Technology study resources

Tamil Nadu HSE Second Year Textile Technology case studies

Tamil Nadu HSE Second Year Textile Technology · Put your knowledge to work in context.

The Tamil Nadu Higher Secondary Examination – Second Year – Textile Technology is a state-board vocational subject paper taken alongside the Plus Two academic subjects. It is intended for students who want a practical, industry-linked qualification rather than a purely academic science stream, and it feeds directly into diploma and degree programmes in textile technology and into entry-level jobs in spinning mills, weaving units, processing houses and garment factories. The Tamil Nadu HSE Second Year Textile Technology case studies are 5 cases and about 3,539 words.

1

Blend Claim on a Handloom Yarn Lot

A handloom cooperative in Karur bought 500 kg of open-end yarn at ₹210/kg, invoiced as 65/35 polyester-cotton. Members complain that the yarn feels harsh, generates static on the warping creel, and takes dye unevenly in their soft-flow machines.

702 words, about 4 min
2

Neps and Noil in a Combed Cotton Mill

A 20,000-spindle spinning mill produces 40s combed hosiery yarn from a mix of Shankar-6 and MCU-5 cotton. For the last eight weeks, the quality report shows card sliver neps of 210 per gram against a normal 90, comber noil of 23.5% against a normal 17%, yarn neps up 280% on the USTER IPI, and end breakage of 38 per 1,000 spindle-hours against a normal 20.

735 words, about 4 min
3

Warp Breakage After a Sizing Change

A powerloom unit has 48 rapier looms weaving a 40s × 40s cotton poplin, 110 ends/inch, 90 picks/inch, 63-inch width. After changing the sizing recipe from a maize-starch/PVA blend to a lower-cost all-maize recipe, warp breakage rose from 1.5 to 3.8 per loom per shift.

694 words, about 3 min
4

Uneven Bleaching and Crease Marks in Cotton Knit Dyeing

A dyehouse processes 1,200 kg/day of 180 gsm cotton single jersey in rope form on two soft-flow machines. The bleaching recipe per litre is 4 g H2O2 (50%), 3 g NaOH, 0.5 g stabilizer, 0.3 g wetting agent, at 98°C for 45 min, liquor ratio 1:8.

670 words, about 3 min
5

Testing Failure on a Navy Poplin Shirt Order

An export house has 5,000 m of 100% cotton poplin, 120 gsm, dyed navy. In-house tests show length shrinkage after one wash at 40°C of 6.5% against a buyer maximum of 3.0%, width shrinkage of 4.2% against 3.0%, colour fastness to rubbing of 3–4 dry against a requirement of 4, and 2–3 wet against a requirement of 3.